Uji Kedalaman Porositas Permukaan Bahan Pit dan Fissure Sealant Berbasis Resin Komposit dan Ionomer Kaca Setelah Direndam Saliva Buatan pH 5,5 (Depth Porosity Test of Surface Materials Pit and Fissure Sealant Based Resin Composite and Glass Ionomer After

  • Annora Ramadhan Fakultas Kedokteran Gigi Universitas Jember
  • Sulistiyani Sulistiyani Fakultas Kedokteran Gigi Universitas Jember
  • Lusi Hidayati Fakultas Kedokteran Gigi Universitas Jember

Abstract


Background. Salivary pH between 5.6 to 7.0 in a normal state. pH below 5.5 included in environments susceptible to caries. Concentration of H+ ions which will outline the high Ca-P bond and will liberate ions into the surrounding environment. So that the material of fissure sealant will lose inorganic mineral constituent and formed on the surface porosity materials. If the sealant surface rough for their porosity can be a retention of plaque and calculus that may cause caries. Other than that, more porosity will affect the compression strength of the material used for fillings when chewing. Purpose. This research purposed to determine the depth of surface porosity difference between pit and fissure sealant materials based resin with glass ionomer after artificial saliva soaked with a pH of 5.5. Method. This research was a laboratory experimental research design with the post test only control group design. The total number of samples required were 16 samples. The tool used a Scanning Electron Microscope (SEM) with units of measurements µ m. Results. The average depth of the material surface porosity pit and fissure sealant resin-based composite of 2.805 μm, while the glass ionomer amounted to 1.912 μm. The surface material pit and fissure sealant resin composite-based artificial saliva soaked with a pH of 5.5 for 24 hours had a depth porosity greater than the surface material pit and fissure sealant glass ionomer-based.


 


Keywords: Depth porosity, glass ionomer, pH 5,5, pit and fissure sealant, resin composite.


 

Published
2017-11-22
How to Cite
RAMADHAN, Annora; SULISTIYANI, Sulistiyani; HIDAYATI, Lusi. Uji Kedalaman Porositas Permukaan Bahan Pit dan Fissure Sealant Berbasis Resin Komposit dan Ionomer Kaca Setelah Direndam Saliva Buatan pH 5,5 (Depth Porosity Test of Surface Materials Pit and Fissure Sealant Based Resin Composite and Glass Ionomer After. Pustaka Kesehatan, [S.l.], v. 5, n. 3, p. 454-460, nov. 2017. ISSN 2721-3218. Available at: <https://jurnal.unej.ac.id/index.php/JPK/article/view/6015>. Date accessed: 27 dec. 2024.
Section
Articles